Nickel Base Alloy yokhala ndi okosijeni komanso kusamva dzimbiri

Kufotokozera Kwachidule:

Mankhwala: NiCr-80/20 Nickel Base Alloy Powder
Mtundu: KF-306
Tinthu Kukula: -140 + 325 mauna, -45 +15 μm
Mtundu: Gasi wa atomized


Tsatanetsatane wa Zamalonda

Zogulitsa Tags

Kugwiritsa ntchito

Nickel base alloy powder ndi zinthu zogwira ntchito kwambiri zomwe zimagwiritsidwa ntchito kwambiri m'mafakitale osiyanasiyana, makamaka m'malo otentha kwambiri komanso owononga.Kukana kwake kwabwino kwa dzimbiri ndi kukana kwa okosijeni kwapamwamba kwambiri kumapangitsa kukhala chisankho chodziwika bwino cha zokutira pazitsulo ndi zitsulo zotsika za alloy pansi pa kutentha kwambiri.Amagwiritsidwanso ntchito ngati gawo lomangirira la zokutira za carbide, zomwe zimapangitsa kukhala chisankho chabwino pazovala zosagwira.

Katundu

Ufawu umapangidwa ndi faifi tambala, chromium, ndi zinthu zina, zomwe zimapangitsa kuti usachite dzimbiri komanso kukhazikika kwa kutentha kwambiri.Ufawu ukhoza kupanga zokutira zomwe zimatha kugwira ntchito kutentha mpaka 980ºC, zomwe zimapangitsa kuti zikhale zoyenera kugwiritsidwa ntchito m'malo ovuta.Chophimbacho chimakhalanso ndi kulimba kwabwino komanso magwiridwe antchito amakina, zomwe zimapangitsa kuti zikhale zoyenera kugwiritsidwa ntchito pazovala zosavala.

Kupanga

Nickel base alloy powder amapangidwa pogwiritsa ntchito mpweya wa atomization.Njirayi imaphatikizapo kusungunula zopangirazo ndikuzipanga kukhala ufa wabwino pogwiritsa ntchito mpweya wothamanga kwambiri.The chifukwa ufa ali yunifolomu tinthu kukula ndi flowability wabwino, zomwe zimapangitsa kuti zikhale zosavuta kusamalira ndi pokonza.

Kugwiritsa ntchito

Nickel base alloy powder amagwiritsidwa ntchito kwambiri m'mafakitale osiyanasiyana, kuphatikiza zakuthambo, kupanga magetsi, ndi kukonza mankhwala.Nthawi zambiri amagwiritsidwa ntchito ngati ❖ kuyanika kuti ateteze zitsulo ndi zitsulo zotsika za alloy zitsulo pansi pa kutentha kwambiri komanso zowonongeka.Amagwiritsidwanso ntchito ngati gawo lomangirira la zokutira za carbide, zomwe zimapangitsa kuti zikhale zoyenera pazovala zosagwira ntchito.Ufawu utha kugwiritsidwa ntchito pogwiritsa ntchito njira zosiyanasiyana zopopera mafuta, kuphatikiza kutsitsi kwa lawi lamoto, kutsitsi kwa plasma, ndi kutsitsi kwamphamvu kwambiri kwa oxy-fuel (HVOF).

Mapeto

Nickel base alloy powder ndi zinthu zogwira ntchito kwambiri zomwe zimagwiritsidwa ntchito kwambiri m'mafakitale osiyanasiyana chifukwa cha kukana kwa dzimbiri komanso kutentha kwambiri kwa okosijeni.The mpweya atomization ndondomeko amaonetsetsa kuti ufa ali yunifolomu tinthu kukula ndi flowability wabwino, kupangitsa kuti zikhale zosavuta kusamalira ndi pokonza.Kukhazikika kwake kwa kutentha kwambiri, kulimba, ndi makina amakina zimapangitsa kukhala chisankho choyenera kugwiritsidwa ntchito m'malo ovuta komanso osagwira ntchito.

Zogulitsa zofanana

Mtundu Dzina lazogulitsa AMPERIT METCO/AMDRY WOKA Mtengo wa PRAXAIR PAC
KF-3061 NiCr-50/50
KF-306 NiCr-80/20 250251 43/5640/4535 NI105/NI106/NI107/1262 98
HastelloyC22
HastelloyC276 409 4276 NDI544/1269 C276
Mtengo wa 718 407 1006 NI202/1278 718
Mtengo wa 625 380 1005 NI328/1265 625

Kufotokozera

Mtundu Dzina lazogulitsa Chemistry (wt%) Kuuma Kutentha Katundu & Kugwiritsa Ntchito
Cr Al W Mo Fe Co Nb Ni
KF-306 NiCr-80/20 20 Bali. Mtengo wa HRC20 ≤980ºC •APS, HVOF Spherical

•Kukana bwino kwa dzimbiri
• Amagwiritsidwa ntchito popanga ma oxidation ndi malaya osagwirizana ndi dzimbiri pa 900 ℃, bond coat pakuyatira pamwamba pa ceramic

Hastelloy 21 3 15 2 2 Bali. Mtengo wa HRC20 ≤900ºC •Kupopera mbewu mankhwalawa pamalo owononga kwambiri
Mtengo wa 718 20 3 18 1 5 Bali. Mtengo wa HRC40 ≤950ºC • Makina opangira gasi
• roketi yamafuta amadzimadzi •Injiniya yotsika kutentha
• Malo okhala ndi asidi •Kupanga zida za nyukiliya
Mtengo wa 625 22 9 5 4 Bali. Mtengo wa HRC20 ≤950ºC •Mayamwidwe nsanja
• Reheater
•Chizindikiro cholowera gasi
•Agitator •Deflector